Real time observation of battery charging/discharing at atomic resolution

Huang et al, Science 330, 1515-1520 (2010) (download pdf , or online version);Read a perspective written by Prof. Yet-Ming Chiang, Science 330, 1485 (2010);Read Nature Materials Editor Dr. Joerg...

View Article



Lithium fiber growth on the anode in a nanowire lithium ion battery during...

Appl. Phys. Lett. 98, 183107 (2011), doi:10.1063/1.3585655 Lithium (Li) dendrite formation has been recognized as one of the major safety concerns for Li metal batteries but not for conventional Li ion...

View Article

Ultrafast Electrochemical Lithiation of Individual Si Nanowire Anodes

Nano Letters, DOI: 10.1021/nl200412p Using advanced in situ transmission electron microscopy, we show that the addition of a carbon coating combined with heavy doping leads to record-high charging...

View Article

Multiple-Stripe Lithiation Mechanism of Individual SnO2 Nanowires in a...

PRL 106, 248302 (2011)    The atomic scale lithiation mechanism of individual SnO2 nanowires in a flooding geometry was revealed by in situ transmission electron microscopy. The lithiation was...

View Article

Anisotropic swelling and fracture of silicon nanowires during lithiation

 Nano Lett. DOI: 10.1021/nl201684d We report direct observation of an unexpected anisotropic swelling of Si nanowires during lithiation against either a solid electrolyte with a lithium...

View Article


Lithiation-Induced Embrittlement of Multiwalled Carbon Nanotubes

ACS Nano, 2011, DOI: 10.1021/nn202071y Lithiation of individual multiwalled carbon nanotubes (MWCNTs) was conducted in situ inside a transmission electron microscope. Upon lithiation, the intertube...

View Article

Reversible nanopore formation in Ge nanowires during lithiation-delithiation...

Nano Lett. 2011, DOI: 10.1021/nl2024118 Retaining the high energy density of rechargeable lithium ion batteries depends critically on the cycle stability of microstructures in electrode materials. We...

View Article

Image may be NSFW.
Clik here to view.

A Beaded-String Silicon Anode

ACS Nano, 2013, 7 (3), pp 2717–2724, DOI: 10.1021/nn4001512 (2013).  Download PDF . Interfacial instability is a fundamental issue in heterostructures ranging from biomaterials to joint replacement and...

View Article


Two dimensional silicon nanowalls for lithium ion batteries

One-dimensional (1-D) nanostructures such as nanowires and nanotubes have been widely explored for anodes with high specific capacity in Li-ion batteries, which effectively release the mechanical...

View Article